Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.660 mm | 0.0260 in | Avg. scar diameter; ASTM D4172 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Four Ball Wear | 0.660 mm | 0.0260 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Unirex PF 500 Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli.. |
|||
Four Ball Wear | 0.660 mm | 0.0260 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Unirex PF 500 Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli.. |
|||
Four Ball Wear | 0.660 mm | 0.0260 in | 40 kg. 1800 rpm, 1- hr at 130°F |
ConocoPhillips 46 FC Fluid-D ISO Description: Conoco FC Fluid-D is a premixed, ready-to-use fluid for hydraulic systems, such as those found in underground-mining equipment that operate where fire-hazard and other personnel safety .. |