Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 299.7 kg
660.8 lb (mass)
Dow Corning MOLYKOTE® G-00050 FG WHITE EP BEARING GREASE
Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning
Four Ball Extreme Pressure, Weld Load 299.7 kg
660.8 lb (mass)
Dow Corning MOLYKOTE® G-0052 FG WHITE EP BEARING GREASE
Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning