Polymer Property : Four Ball Extreme Pressure, Weld Load = 160 kg Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2783
ExxonMobil 24 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2596
ExxonMobil Unirex S 2
Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2596, DIN 51 350/4
Chesterton 601 Chain Drive Pin & Bushing Lubricant
Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
kgf; ASTM D2783
ChevronTexaco Pinnacle® 220
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
kgf; ASTM D2783
ChevronTexaco Pinnacle® 680
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2596
ExxonMobil Unirex S 2
Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6068 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6320 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6460 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6680 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 15 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 150 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 460 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2783
ExxonMobil 24 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 68 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 10 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ConocoPhillips Hydroclear® 320 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
kgf; ASTM D2783
ChevronTexaco Pinnacle® 320
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
kgf; ASTM D2783
ChevronTexaco Pinnacle® 460
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
ConocoPhillips ANDEROL® 6150 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D2266, DIN 51 350
Chesterton 652 Pneumatic Lubricant & Conditioner
Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e..