Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | ISO 180 |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | ISO 180-A |
Ecomass® 1950TU76 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Polyamide (PA6/10)Very Good ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L PA66 D61 PA66, Injection Molded Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 TF POM Tribological modified grade low level addition of PTFE, which lower coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched (ISO) | 6.30 kJ/m² | 3.00 ft-lb/in² | ISO 180 |
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |