Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.20 - 22.0 kJ/m² | 2.95 - 10.5 ft-lb/in² | Average value: 12.0 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Izod Impact, Notched (ISO) | 6.20 kJ/m² | 2.95 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF33-66/6 XE-BK167A 33% Glass Filled, Color Matched Ebony Nylon 66/6 Description: Glass Filled, Color Matched Ebony Nylon 66/6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 6.20 kJ/m² | 2.95 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 SI POM Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |