Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 97.0 kJ/m² @Temperature -50.0 °C |
46.2 ft-lb/in² @Temperature -58.0 °F |
|
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good proces.. |