Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and goo.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS PC+ ABS General Purpose Non-FR |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9612G PC (Asia Pacific) Lexan LUX9612G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND HI 10 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents. Main application fields: autom.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 0.000 °C |
19.0 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength 20% Mineral Reinforced, Very High Stiffness & Very High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1627-GY1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO Test |
BASF Ultramid® B29 HM 01 PA6 (Dry) Ultramid B29 HM 01 is a medium viscosity , heat stabilized, PA6 universal wire jacketing resin offering excellent performance through the range of THHN, THWN, and TFFN constructions. It possesses a.. |
|||
Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |