Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.70 kJ/m² | 2.24 ft-lb/in² | ISO 180 |
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man.. |
|||
Izod Impact, Notched (ISO) | 4.70 kJ/m² | 2.24 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application.. |
|||
Izod Impact, Notched (ISO) | 4.70 kJ/m² @Temperature -20.0 °C |
2.24 ft-lb/in² @Temperature -4.00 °F |
ASTM D256 |
C.O.I.M. LARIPUR® LPR6325 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Izod Impact, Notched (ISO) | 4.70 kJ/m² | 2.24 ft-lb/in² | ISO Test |
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Izod Impact, Notched (ISO) | 4.70 kJ/m² | 2.24 ft-lb/in² | ISO Test |
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |