Polymer Property : Izod Impact, Notched (ISO) = 3.38 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.10 - 79.0 kJ/m²
3.38 - 37.6 ft-lb/in²
Average value: 18.9 kJ/m² Grade Count:57
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched (ISO) 7.10 kJ/m²
3.38 ft-lb/in²
ISO 180-1A
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 7.10 kJ/m²
3.38 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 GF5 POM
26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Izod Impact, Notched (ISO) 7.10 kJ/m²
3.38 ft-lb/in²
ISO 180
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..