Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 - 22.0 kJ/m² @Temperature -40.0 - -30.0 °C |
1.43 - 10.5 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 7.20 kJ/m² Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 22.0 kJ/m² @Temperature -30.0 - -20.0 °C |
3.33 - 10.5 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 13.1 kJ/m² Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 6.20 - 22.0 kJ/m² | 2.95 - 10.5 ft-lb/in² | Average value: 12.0 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |