Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 2.24 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.70 kJ/m²
2.24 ft-lb/in²
ISO 180
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man..
Izod Impact, Notched (ISO) 4.70 kJ/m²
2.24 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
Izod Impact, Notched (ISO) 4.70 kJ/m²

@Temperature -20.0 °C
2.24 ft-lb/in²

@Temperature -4.00 °F
ASTM D256
C.O.I.M. LARIPUR® LPR6325 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Izod Impact, Notched (ISO) 4.70 kJ/m²
2.24 ft-lb/in²
ISO Test
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT
Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
Izod Impact, Notched (ISO) 4.70 kJ/m²
2.24 ft-lb/in²
ISO Test
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000.
Copyright © lookpolymers.com All Rights Reserved