Polymer Property : Izod Impact, Notched (ISO) = 19.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 41.0 kJ/m²

@Temperature -30.0 °C
19.5 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS
Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific)
Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
Izod Impact, Notched (ISO) 41.0 kJ/m²
19.5 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.