Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Izod Impact, Notched (ISO) 19.1 kJ/m²
9.09 ft-lb/in²
ISO 180
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..