Polymer Property : Izod Impact, Notched (ISO) = 1.24 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.60 - 9.00 kJ/m²
1.24 - 4.28 ft-lb/in²
Average value: 6.18 kJ/m² Grade Count:20
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Izod Impact, Notched (ISO) 2.60 - 15.0 kJ/m²

@Temperature -20.0 - -20.0 °C
1.24 - 7.14 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 5.34 kJ/m² Grade Count:13
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Izod Impact, Notched (ISO) 2.60 - 15.0 kJ/m²
1.24 - 7.14 ft-lb/in²
Average value: 7.65 kJ/m² Grade Count:18
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Izod Impact, Notched (ISO) 2.60 - 16.0 kJ/m²
1.24 - 7.61 ft-lb/in²
Average value: 5.20 kJ/m² Grade Count:31
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
ISO 180-1A
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Izod Impact, Notched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
ISO 180-93
Wellman EcoLon® MRGF1518-BK3 38% Mineral/Glass Reinforced Post Consumer Compound Nylon 66
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman.
Izod Impact, Notched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
ISO 180-93
Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66
Description: Glass Sphere Reinforced, Natural Nylon 66Information provided by Wellman.