Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² - NB | 45.7 ft-lb/in² - NB | Average value: 97.0 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² | 45.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² | 45.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² | 45.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific) High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 96.0 kJ/m² @Temperature 23.0 °C |
45.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |