Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific) LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 94.0 kJ/m² | 44.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific) LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber. |