Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 9.50 - 9.50 kJ/m² @Temperature -40.0 - -40.0 °C |
4.52 - 4.52 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 9.50 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Unnotched (ISO) | 9.50 - 9.50 kJ/m² @Temperature -40.0 - -40.0 °C |
4.52 - 4.52 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 9.50 kJ/m² Grade Count:1 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Unnotched (ISO) | 9.50 kJ/m² @Temperature -40.0 °C |
4.52 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DSM Akulon® M-1016 (Dry) 33% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Izod Impact, Unnotched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NTJA Homopolymer 30% Talc Filled Polypropylene Information provided by A.D. Compound |