Polymer Property : Izod Impact, Unnotched (ISO) = 32.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 40.0 - 68.0 kJ/m²
19.0 - 32.4 ft-lb/in²
Average value: 50.7 kJ/m² Grade Count:13
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Izod Impact, Unnotched (ISO) 18.0 - 68.0 kJ/m²

@Temperature -45.0 - -30.0 °C
8.57 - 32.4 ft-lb/in²

@Temperature -49.0 - -22.0 °F
Average value: 42.8 kJ/m² Grade Count:6
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..