Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.0 - 30.0 kJ/m² @Temperature -30.0 - -30.0 °C |
14.3 - 14.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 30.0 kJ/m² Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |