Polymer Property : Izod Impact, Unnotched (ISO) = 23.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC
LNP* LUBRICOMP* DFP36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²

@Temperature 23.0 °C
23.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC
LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
Type 1; ISO 180
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Izod Impact, Unnotched (ISO) 49.0 kJ/m²

@Temperature 23.0 °C
23.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal
LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK
LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66
LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006S PP
LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific)
LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East)
LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006SU PP
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA6.10
LNP* LUBRICOMP* QCP36 is a compound based on Nylon 6/10 resin containing 15% PTFE/Silicone, 30% Carbon Fiber. Added features of this material include: Wear Resistant. Electrically Conductive
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
Type 1; ISO 180
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti..
Copyright © lookpolymers.com All Rights Reserved