Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 17.0 - 57.0 kJ/m² | 8.09 - 27.1 ft-lb/in² | Average value: 36.9 kJ/m² Grade Count:19 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 - 24.0 kJ/m² @Temperature -30.0 - -30.0 °C |
8.09 - 11.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 20.5 kJ/m² Grade Count:2 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific) LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF006AS PP LNP THERMOCOMP* MF006AS is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP ZX08005 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZX08005 is a Compound based on PPE + PS Blend resin, containing Mineral. Added features include: Improved Dielectric Properties. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ASTM D256 |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ASTM D256 |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide 6 80E7 PA6, Injection Molded Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | ISO 180 |
Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber Reinforced with glass fiber and minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |