Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11
LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific)
LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11
LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP
LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched
LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched
LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
Izod Impact, Unnotched (ISO) 13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear
LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East)
NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East)
NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306.
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1U
A.D. Compound Adene NTTAG Copolymer 40% Talc Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Unnotched (ISO) 13.0 - 13.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.19 - 6.19 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.0 kJ/m² Grade Count:1
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 171 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high ..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1U
A.D. Compound Adene NCHA Homopolymer 25% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Unnotched (ISO) 13.0 kJ/m² - NB

@Temperature -30.0 - -30.0 °C
6.19 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 50.3 kJ/m² Grade Count:175
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Izod Impact, Unnotched (ISO) 13.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.19 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 27.3 kJ/m² Grade Count:6
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has ..
Izod Impact, Unnotched (ISO) 13.0 kJ/m²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has ..