Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 125 kJ/m² | 59.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP COLORCOMP W10009I PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* W10009I is a compound based on Polybutylene Terephalate resin containing Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 125 kJ/m² | 59.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East) LNP* LUBRICOMP* PI001 is a compound based on PA 6 resin containing Silicone. Added features include Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 125 kJ/m² | 59.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Izod Impact, Unnotched (ISO) | 125 kJ/m² | 59.5 ft-lb/in² | ISO 180/1C |
Chi Mei Polylac® PA-777D ABS - High Heat Super High Heat |