Polymer Property : Adhesive Bond Strength = 754 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.20 MPa

@Temperature 93.0 °C
754 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9330.3 Paste Adhesive System
Non-slump, thixotropic adhesive with high peel strength and excellent environmental durability.Applications:Structural Repair Composite Bonding
Adhesive Bond Strength 5.20 MPa

@Temperature 93.0 °C
754 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9309.3NA Paste Adhesive System
Toughened adhesive with excellent peel strength. Contains glass beads for bond line control.Applications: Structural Repair Composite Bonding
Adhesive Bond Strength 5.20 MPa

@Temperature 93.0 °C
754 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9330 Paste Adhesive System
Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding