Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories AMCM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories AMCM-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ASCM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ASCM-S Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories GM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | <= 4.905 MPa @Temperature 500 °C, Time 10800 sec |
<= 711.4 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories HM-S Special Mortar for Sliding Gate Valve Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1400 °C, Time 10800 sec |
711.4 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories SCH-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 1000 °C, Time 10800 sec |
711.4 psi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SP-60W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 110 °C, Time 86400 sec |
711.4 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SP-70W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 500 °C, Time 10800 sec |
711.4 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories SP-85W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 4.905 MPa @Temperature 110 °C, Time 86400 sec |
711.4 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SP-85W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |