Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories AMCM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories AMCM-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories ASCM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories ASCM-S Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories GM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength <= 4.905 MPa

@Temperature 500 °C,
Time 10800 sec
<= 711.4 psi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories HM-S Special Mortar for Sliding Gate Valve
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1400 °C,
Time 10800 sec
711.4 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories SCH-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 1000 °C,
Time 10800 sec
711.4 psi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SP-60W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 110 °C,
Time 86400 sec
711.4 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SP-70W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 500 °C,
Time 10800 sec
711.4 psi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories SP-85W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 4.905 MPa

@Temperature 110 °C,
Time 86400 sec
711.4 psi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SP-85W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).