Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.9 MPa @Temperature 25.0 °C |
2300 psi @Temperature 77.0 °F |
Lap Shear Strength vs. Aluminum |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |