Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.9 MPa @Temperature -55.0 °C |
2310 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9377 Paste Adhesive System Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 25.0 °C |
2310 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9377 Paste Adhesive System Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim |
|||
Adhesive Bond Strength | 15.9 MPa @Thickness 0.750 mm |
2310 psi @Thickness 0.0295 in |
Lap Shear (CRS St 1203); EN 1465 |
Dow BETAMATE™ XW 1185 Epoxy BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi.. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 25.0 °C |
2300 psi @Temperature 77.0 °F |
Lap Shear Strength vs. Aluminum |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 177 °C |
2310 psi @Temperature 351 °F |
Lap Shear |
Henkel Hysol EA 9657 Film Adhesive High temperature, service film adhesive designed for high honeycomb peel in a reticulated sound suppression structure. Qualified to BMS 5-137. Data from .080 psf, 400 g / m2.Applications: Composite .. |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature -55.0 °C |
2310 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9395 Paste Adhesive System Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 15.9 MPa @Temperature 25.0 °C |
2310 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 956 Paste Adhesive System Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up |