Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 6.90 MPa @Temperature 25.0 °C |
1000 psi @Temperature 77.0 °F |
tube shears |
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive Modified BMI foaming core splice, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs. Elevated service temperature to 450°F / 232°C. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 121 °C |
1000 psi @Temperature 250 °F |
tube shears |
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive Modified BMI foaming core splice, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs. Elevated service temperature to 450°F / 232°C. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 121 °C |
1000 psi @Temperature 250 °F |
tube shears |
Henkel Hysol MA 562S Core Splice Adhesive Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Nonmetallic, medium tack, excellent slump resistance. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 93.0 °C |
1000 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9359.3 Paste Adhesive System Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 93.0 °C |
1000 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9360 Paste Adhesive System Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 93.0 °C |
1000 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9320NA Paste Adhesive System High shear and high peel adhesive system with room temperature cure. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 149 °C |
1000 psi @Temperature 300 °F |
Lap Shear |
Henkel Hysol EA 9686 Film Adhesive Second generation, moisture resistant, toughened 250°F / 121°C curing film with service performance to 300°F / 149°C. Excellent for composite or metal bonding. Data from .060 psf, 300 g / m2.App.. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 121 °C |
1000 psi @Temperature 250 °F |
tube shears |
Henkel Hysol MA 562SFR Core Splice Adhesive Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Flame-retardant, nonmetallic, medium tack, excellent slump resistance. |