Polymer Property : Charpy Impact Unnotched = 8.30 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.30 J/cm²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..
Charpy Impact Unnotched 8.30 J/cm²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher..
Charpy Impact Unnotched 8.30 J/cm²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1017GH33 BK701 PA6-GF33
33% Glass Reinforced, Heat Stabilized, Injection Molding
Charpy Impact Unnotched 8.30 J/cm²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 8.30 J/cm²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber
SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com..