Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 7.20 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.20 J/cm²

@Temperature 23.0 °C
34.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized
15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
Charpy Impact Unnotched 7.20 J/cm²

@Temperature -30.0 °C
34.3 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 7.20 J/cm²

@Temperature 23.0 °C
34.3 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 7.20 J/cm²

@Temperature 23.0 °C
34.3 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved