Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -20.0 °C |
41.4 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature 23.0 °C |
41.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com.. |