Polymer Property : Charpy Impact Unnotched = 3.90 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -20.0 °C
18.6 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -20.0 °C
18.6 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre
FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -20.0 °C
18.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A RV150 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop.
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -20.0 °C
18.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -20.0 °C
18.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH GF8030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15
15% Glass Reinforced, Heat Stabilized, Injection Molding
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon  (Unverified Data**)
Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by Du..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -30.0 °C
18.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Charpy Impact Unnotched 3.90 J/cm²

@Temperature -30.0 °C
18.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled
SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers