Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -20.0 °C
24.7 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 49 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -20.0 °C
24.7 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 49 GF 50 Polypropylene Homopolymer, 50% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 50% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -20.0 °C
24.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® A RV250AF (cond.) Nylon 66-25GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RCV3515 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -20.0 °C
24.7 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -20.0 °C
24.7 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 49 GF 30 LW PP, 30% glass fibre, coupling agents, laser writer
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties and contains modificator for laser labeling of fini..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RCP3010LK (cond.) Nylon 6
PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group.
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate
SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
Copyright © lookpolymers.com All Rights Reserved