Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling
FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® A RV300AF (dry) Nylon 66-30GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX2415 PC
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer
Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 4.70 J/cm²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1fU
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1fU
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature 23.0 °C
22.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact Unnotched 4.70 J/cm²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...