Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 15 FRG 2 LW PA6, 15% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 960°..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling
FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers
Charpy Impact Unnotched 4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..