Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -20.0 °C |
12.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 GF 20 002 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 20% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -20.0 °C |
12.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -20.0 °C |
12.8 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -20.0 °C |
12.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 25 Polyamide 6, 25% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 25% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
DIN 53453 |
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-3130 is a 30% talc-filled polypropylene homopolymer compound /PP-H TD30 (ISO 1043)/. This grade is available in natural and custom colored form as well.INNOPOL® CS 1-3130 is reco.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX5121 PBT (Europe-Africa-Middle East) VALOX VX5121 is a 15 % glass reinforced PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |