Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 2.20 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 51 T 40 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 40% mineral filler. General application. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -20.0 °C
10.5 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PQ 83 T 30 Polypropylene reinforced with mineral filler
Impact modified PP for injection molding with the content of 30 % mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o.
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -20.0 °C
10.5 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur..
Charpy Impact Unnotched 2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -30.0 °C
10.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2520 L POM
Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -20.0 °C
10.5 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
Charpy Impact Unnotched 2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -20.0 °C
10.5 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.20 J/cm²

@Temperature -40.0 °C
10.5 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Copyright © lookpolymers.com All Rights Reserved