Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LATAN 13 S/30 30% Glass Sphere Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-3000 N DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 N DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 108 GF17 Acrylonitrile Butadiene Styrene, 17% Glass Fiber Saxalac 108 GF17 is a 17% glass fiber reinforced ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data te.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat.. |