Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.800 - 1.40 J/cm²

@Temperature 23.0 °C
3.81 - 6.66 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Charpy Impact Unnotched 0.800 - 1.30 J/cm²

@Temperature 23.0 °C
3.81 - 6.19 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact Unnotched 0.800 - 1.40 J/cm²

@Temperature 23.0 °C
3.81 - 6.66 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Charpy Impact Unnotched 0.800 - 1.10 J/cm²

@Temperature 23.0 °C
3.81 - 5.24 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group RALUPOL® 4385 UP
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy..
Charpy Impact Unnotched 0.800 - 1.10 J/cm²

@Temperature 23.0 °C
3.81 - 5.24 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Charpy Impact Unnotched 0.800 J/cm²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound  (Unverified Data**)
Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us..
Charpy Impact Unnotched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri..
Charpy Impact Unnotched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Charpy Impact Unnotched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
ASTM DIN53453
Total PPC 4280W Polypropylene, Impact Copolymer
ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hard..