Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1105-8173 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 20-0664 Polyphthalamide, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1-7139-1 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1-7984 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7918 PEEK, unreinforced Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss LUVOCOM® 1-8227 Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Tensile Stress | 80.0 MPa | 11600 psi | |
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann .. |