Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 75.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 75.0 MPa
10900 psi
Akro-Plastic Akromid® B3 3 S3 10 PA, Dry-Impact Resistant  (Unverified Data**)
The product types are mainly used in the automobile industry sector, but also for the domestic industry, the building industry and the leisure time-and sporting goods industry, AKROMID has become a ..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-7568/GY PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Superheated steam sterilizable.High chemical resistance parts, hydrolysis resistance, non ..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally..
Tensile Stress 75.0 MPa
10900 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1502-7865/BK2 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 75.0 MPa
10900 psi
Lehmann & Voss LUVOCOM® 80-8030 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Tensile Stress 75.0 MPa
10900 psi
ISO 527-2
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS)
Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch..
Tensile Stress 75.0 MPa
10900 psi
ISO 527-2
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS)
Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista..
Copyright © lookpolymers.com All Rights Reserved