Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1823 AS Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL EF-6109 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |