Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 320 MPa | 46400 psi | |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Tensile Stress | 320 MPa | 46400 psi | |
Lehmann & Voss LUVOCOM® 1/XCF/40 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Tensile Stress | 320 MPa | 46400 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Tensile Stress | 320 MPa | 46400 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |