Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 28.0 MPa | 4060 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Tensile Stress | 28.0 MPa | 4060 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Tensile Stress | 28.0 MPa | 4060 psi | ISO R527 |
Iran Petrochemical (PCC) EP2 X 49 GA Polypropylene This grade features extremely high flow properties, excellent transparency and high gloss.Applications: Crouse holds containers, video cassette boxes, packaging for food, cosmetics.Information provi.. |
|||
Tensile Stress | 28.0 MPa | 4060 psi | ISO R527 |
Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antist.. |