Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |