Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 32.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 32.0 MPa
4640 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene
BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su..
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene
BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo..
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene
EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.Applications: stretched film and tapes for prod..
Tensile Stress 32.0 MPa
4640 psi
ASTM D638
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene
Moplen Z 30 G is a high flow homopolymer for injection molding and compounding applications. Moplen Z 30 G exhibits a high stiffness and an outstanding processability for shorter cycle times and eas..
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene
BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c..
Tensile Stress 32.0 MPa
4640 psi
Break, (50mm/min); ISO 527-2, -1A
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..
Tensile Stress 32.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
4640 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..