Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1486A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1564F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1862R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2320 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-75M200 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated with high flow properties and exc.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |