Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.27 MPa @Strain 100 % |
329 psi @Strain 100 % |
|
NEU Neuthane N8511-1H Aromatic, Polyester TPU Blend A blend of aromatic, polyester TPUs with good clarity |