Polymer Property : Tensile Stress = 120 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 50/CF/10/GF/10/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 50-7644 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f..
Tensile Stress 120 MPa
17400 psi
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Tensile Stress 120 MPa
17400 psi
Akro-Plastic Akromid® B3 GF 15 S1 PA, Cold-Impact Resistant  (Unverified Data**)
The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio..
Tensile Stress 120 MPa
17400 psi
Akro-Plastic Akromid® B3 GF 15 S3 PA, Dry-Impact Resistant, 15% Glass Filled  (discontinued **)
The product types are mainly used in the automobile industry sector, but also for the domestic industry, the building industry and the leisure time-and sporting goods industry, AKROMID has become a ..